Best Outstanding Achievement Award
"Development of broadly wavelength swept pulsed QCL"
Outstanding Achievement Awards
"Analysis on degradation of mechanical property of ceramics zirconia"
"Development of advanced functional materials for next-generation semiconductor wiring bonding materials"
"Giant dielectric constant in Al2O3/TiO2 multilayer films synthesized by ALD"
"Collection of urine extracellular vesicles via nanowires"
nano tech 2019 Poster Exhibition
1. Analysis on degradation of mechanical property of ceramics zirconia
2. Development of advanced functional materials for next-generation semiconductor wiring bonding materials
3. Giant dielectric constant in Al2O3/TiO2 multilayer films synthesized by ALD
4. Development of broadly wavelength swept pulsed QCL
5. Collection of urine extracellular vesicles via nanowires
*Click each image to download a PDF file.