利用報告書 / User's Reports

  • 印刷する

【公開日:2023.08.01】【最終更新日:2023.05.02】

課題データ / Project Data

課題番号 / Project Issue Number

22KU1031

利用課題名 / Title

可食性成分を用いた青果物鮮度保持コーティング剤の開発

利用した実施機関 / Support Institute

九州大学 / Kyushu Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)物質・材料合成プロセス/Molecule & Material Synthesis(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マルチマテリアル化技術・次世代高分子マテリアル/Multi-material technologies / Next-generation high-molecular materials(副 / Sub)次世代ナノスケールマテリアル/Next-generation nanoscale materials

キーワード / Keywords

コンポジット材料/ Composite material


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

田中 良奈

所属名 / Affiliation

九州大学大学院農学研究院

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Ata Aditya Wardana

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

KU-513:ゼータ電位・粒径・分子量測定装置群


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

A breakthrough for antifungal coating production through hydroxypropyl cellulose (HPC), lauric arginate (charged emulsifier) (LAE), and cinnamaldehyde (CDH) was developed. It was made from 2% HPC, 0.2% LAE and 0.3% CDH. The incorporation of LAE and may improve the performance of HPC antifungal activities additively confirmed with a series of assays (in vitro, in vivo, and membrane integrity changes)

実験 / Experimental

Each coating solution was measured for zeta potential value by using a Zetasizer (Zetasizer Nano ZNP, Malvern Instruments, UK) with five replications.

結果と考察 / Results and Discussion

Zeta potential value of all coating solutions showed negatively charged surfaces ( -1.31 for HPC, and -3.24 for HPC/CDH), except for HPC/CDH containing LAE (10.47).. Theoretically, zeta potential value more than ±30 mV (negative or positive) represented the physically stable dispersions as the result of electrostatic repulsion (Kringel et al., 2019).  The addition of LAE increased zeta potential value of Chi dramatically (P

図・表・数式 / Figures, Tables and Equations


Zeta potential value of HPC/LAE/CDH (a), HPC (b), and HPC/CDH (c)


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る