【公開日:2024.07.25】【最終更新日:2024.03.28】
課題データ / Project Data
課題番号 / Project Issue Number
23NM5426
利用課題名 / Title
Synthesis and Integration of 2D materials for high-performance
利用した実施機関 / Support Institute
物質・材料研究機構 / NIMS
機関外・機関内の利用 / External or Internal Use
内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)
ARIM半導体基盤PF関連課題 / Related to ARIM-SETI
指定なし/No Designation
技術領域 / Technology Area
【横断技術領域 / Cross-Technology Area】(主 / Main)加工・デバイスプロセス/Nanofabrication(副 / Sub)-
【重要技術領域 / Important Technology Area】(主 / Main)量子・電子制御により革新的な機能を発現するマテリアル/Materials using quantum and electronic control to perform innovative functions(副 / Sub)-
キーワード / Keywords
Transistors, Chemical Vapor Deposition (CVD), 1D Nanoribbons, 2D Materials
利用者と利用形態 / User and Support Type
利用者名(課題申請者)/ User Name (Project Applicant)
Shisheng LI
所属名 / Affiliation
物質・材料研究機構
共同利用者氏名 / Names of Collaborators Excluding Supporters in the Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Supporters in the Hub and Spoke Institutes
利用形態 / Support Type
(主 / Main)機器利用/Equipment Utilization(副 / Sub)-
利用した主な設備 / Equipment Used in This Project
NM-605:水蒸気プラズマ洗浄装置 [AQ-500 #1]
NM-606:UVオゾンクリーナー [UV-1]
NM-612:SiNプラズマCVD装置 [PD-220NL]
NM-649:FE-SEM+EDX [SU8230]
報告書データ / Report
概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)
The AFM and SEM are high-efficiency tools for studying the morphology of CVD-grown materials including the information on thickness, length, width, etc.
実験 / Experimental
AFM tapping mode and SEM were employed to study the morphology of as-grown 1D MoS2 nanoribbons grown on mechanically exfoliated h-BN flakes.
結果と考察 / Results and Discussion
AFM images of the as-grown 1D MoS2 nanoribbons have sharp and straight edges. The thickness of the MoS2 nanoribbon is ~0.7 nm, indicating a monolayer thickness. Since the Jupiter XR AFM can achieve the atomic resolution. It is promising to study the epitaxy relationship between the top MoS2 nanoribbon and bottom h-BN flakes in the future. SEM images show morphology at a large scope which can easily tell the length of the as-grown 1D MoS2 nanoribbons and how the width evolves during the growth process. Because of the precipitation of MoS2 from the Na-Mo-O-S droplets, the width of 1D MoS2 nanoribbons shrinks gradually.
図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)
成果発表・成果利用 / Publication and Patents
論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents
特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件