利用報告書 / User's Reports

  • 印刷する

【公開日:2025.06.10】【最終更新日:2025.04.05】

課題データ / Project Data

課題番号 / Project Issue Number

24NM5086

利用課題名 / Title

Application of LaB6 nanowire emitter

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マテリアルの高度循環のための技術/Advanced materials recycling technologies(副 / Sub)-

キーワード / Keywords


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

張 晗

所属名 / Affiliation

物質・材料研究機構

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

山内 陽介

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NM-510:FIB加工装置(JIB-4000)


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

I use LaB6 nanowires to fabricate electron emitters for electron microscope use. The fabrication process involves using FIB to modify the shape a Ta needle. After the special shape is made on the Ta needle tip, LaB6 nanowires could be attached to such tip to realize an electron emitter.

実験 / Experimental

Using JIB-4000, FIB milling was performed at two locations on the tip of the Ta needle from two different angles.

結果と考察 / Results and Discussion

We succeeded in milling a Ta needle (Fig.1) using FIB and processing it into a shape suitable for attaching LaB6 nanowires (Fig.2 and 3). With JIB-4000, we were able to perform accurate cutting from 5 μm to 20 μm and sufficient surface smoothing.

図・表・数式 / Figures, Tables and Equations


Fig.1 Ta needle before processing



Fig.2 FIB image of Ta needle during processing



Fig.3 FIB image of Ta needle after processing


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)

This work was supported by NIMS Electron Microscopy Analysis Station, Nanostructural Characterization Group.


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)