【公開日:2024.07.25】【最終更新日:2025.05.20】
課題データ / Project Data
課題番号 / Project Issue Number
23AE0004
利用課題名 / Title
In-situ XAFS study of noble metal high entropy alloy nanoparticles with high stable and excellent activity under CO oxidation conditions
利用した実施機関 / Support Institute
日本原子力研究開発機構 / JAEA
機関外・機関内の利用 / External or Internal Use
外部利用/External Use
技術領域 / Technology Area
【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-
【重要技術領域 / Important Technology Area】(主 / Main)革新的なエネルギー変換を可能とするマテリアル/Materials enabling innovative energy conversion(副 / Sub)-
キーワード / Keywords
XAFS, high-entropy alloy, CO oxidation, catalysts
利用者と利用形態 / User and Support Type
利用者名(課題申請者)/ User Name (Project Applicant)
Wu Dongshuang
所属名 / Affiliation
Nanyang Technological University
共同利用者氏名 / Names of Collaborators Excluding Supporters in the Hub and Spoke Institutes
O. Seo,O. Sakata,J. Tang,Y. Wang,H. Gu
ARIM実施機関支援担当者 / Names of Supporters in the Hub and Spoke Institutes
松村 大樹
利用形態 / Support Type
(主 / Main)共同研究/Joint Research(副 / Sub)-
利用した主な設備 / Equipment Used in This Project
報告書データ / Report
概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)
The purpose of this beam time is to observe the electronic structure change of metal alloy nanoparticles from monometallic to high-entropy alloy nanoparticles during the gas atmosphere.
実験 / Experimental
First, we observed the ex situ XAFS of the samples in the pellet form. For the in situ measurement, focusing on the In K-edge and Mn K-edge, the samples were pressurized and fitted into the in situ holder provided by Dr. Matsumura. The XAFS spectra were obtained under different atmospheres including vacuum, H2 (1 bar and 9 bar), CO2 (1 bar and 9 bar) with varying temperatures (RT to 773 K).
結果と考察 / Results and Discussion
During this beamtime, we have confirmed that all the liquid metal-based nanoparticles are covered by metal oxide layers on their surfaces. The thickness of the surface oxide layers is highly dependent on the particle size. Small NPs have thicker layers. We also found that the formed oxide layers have shorter M-O bond lengths than their corresponding crystalline metal oxides. These results are in line with the XPS as well as the XRD results. As for the liquid metal loaded on support, we found that the liquid metal tends to get lattice oxygen from the supported metal oxides and forms the amorphous liquid metal oxides. We also find that the coordination of metals is changed by changing the gas atmosphere. Moreover, MnO2 was found to be unstable during the CO2 and H2 atmospheres. With a long-term gas phase treatment, MnCO3 was found. This suggests the activity of MnO2 for CO2 hydrogenation but also the instability.
図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)
成果発表・成果利用 / Publication and Patents
論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
-
Bing Zhu, Stabilizing the Unstable: Enhancing OER Durability with 3d-Orbital Transition Metal Multielemental Alloy Nanoparticles by Atomically Dispersed 4d-Orbital Pd for a 100-Fold Extended Lifetime, Journal of the American Chemical Society, 147, 11250-11256(2025).
DOI: https://pubs.acs.org/doi/full/10.1021/jacs.4c18109
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents
特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件