利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.03.28】

課題データ / Project Data

課題番号 / Project Issue Number

23NM5426

利用課題名 / Title

Synthesis and Integration of 2D materials for high-performance

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)加工・デバイスプロセス/Nanofabrication(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)量子・電子制御により革新的な機能を発現するマテリアル/Materials using quantum and electronic control to perform innovative functions(副 / Sub)-

キーワード / Keywords

Transistors, Chemical Vapor Deposition (CVD), 1D Nanoribbons, 2D Materials


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Shisheng LI

所属名 / Affiliation

物質・材料研究機構

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NM-605:水蒸気プラズマ洗浄装置 [AQ-500 #1]
NM-606:UVオゾンクリーナー [UV-1]
NM-612:SiNプラズマCVD装置 [PD-220NL]
NM-649:FE-SEM+EDX [SU8230]


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

The AFM and SEM are high-efficiency tools for studying the morphology of CVD-grown materials including the information on thickness, length, width, etc.

実験 / Experimental

AFM tapping mode and SEM were employed to study the morphology of as-grown 1D MoS2 nanoribbons grown on mechanically exfoliated h-BN flakes.

結果と考察 / Results and Discussion

AFM images of the as-grown 1D MoS2 nanoribbons have sharp and straight edges. The thickness of the MoS2 nanoribbon is ~0.7 nm, indicating a monolayer thickness. Since the Jupiter XR AFM can achieve the atomic resolution. It is promising to study the epitaxy relationship between the top MoS2 nanoribbon and bottom h-BN flakes in the future. SEM images show morphology at a large scope which can easily tell the length of the as-grown 1D MoS2 nanoribbons and how the width evolves during the growth process. Because of the precipitation of MoS2 from the Na-Mo-O-S droplets, the width of 1D MoS2 nanoribbons shrinks gradually. 

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

  • 【更新日】0年0月0日
印刷する
PAGE TOP
スマートフォン用ページで見る