利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.06.22】

課題データ / Project Data

課題番号 / Project Issue Number

23NU0249

利用課題名 / Title

Semiconductor photocatalysis

利用した実施機関 / Support Institute

名古屋大学 / Nagoya Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マテリアルの高度循環のための技術/Advanced materials recycling technologies(副 / Sub)-

キーワード / Keywords

電子スピン共鳴, ESR, YTOS,資源代替技術/ Resource alternative technology


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Yaqiang WU

所属名 / Affiliation

名古屋大学大学院工学研究科

共同利用者氏名 / Names of Collaborators Excluding Supporters in the Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Supporters in the Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

NU-236:In-situ電子スピン共鳴


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

Employ electron spin resonance (ESR) test to study the defects in YTOSsamples, mainly including O vacancies and Ti3+ species. These defects affected by heating time during the preparation process of  YTOS were discessed here.

実験 / Experimental

YTOS powder samples prepared from differen heating durations were weighed, recoreded, and added into nuclear magnetic tubs for ESR testment. Obtiaend signal data were recorded.

結果と考察 / Results and Discussion

The electron spin resonance (ESR) was performed to study the defects in Y2Ti2O5S2 (YTOS) samples with different synthetic procedures. As for the SSR samples, O vacancy was detected at 3514 G (g=2.01) and the signal intensity was increased with decreasing the heating duration. In the case of Flux-1/y samples, no obvious O vacancy signal was observed, but the signals for Ti3+ were observed at 3600 and 3680 G (g=1.96 and 1.92, respectively), and the signal strength was decreased with the decrease in the heating duration. 

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)

Reference:Angew. Chem. Int. Ed. 2023, 62, e202310607


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
  1. Lihua Lin, Flux‐Assisted Synthesis of Y2Ti2O5S2 for Photocatalytic Hydrogen and Oxygen Evolution Reactions, Angewandte Chemie International Edition, 62, (2023).
    DOI: 10.1002/anie.202310607
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

印刷する
PAGE TOP
スマートフォン用ページで見る