利用課題名 / Title

エレクトロクロミック調光ガラスデバイス開発

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)加工・デバイスプロセス/Nanofabrication(副 / Sub)計測・分析/Advanced Characterization

【重要技術領域 / Important Technology Area】(主 / Main)量子・電子制御により革新的な機能を発現するマテリアル/Materials using quantum and electronic control to perform innovative functions(副 / Sub)-

キーワード / Keywords

Electronic device, Thin films, Powered Electronics,電子顕微鏡/ Electronic microscope,リソグラフィ/ Lithography


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

樋口 昌芳

所属名 / Affiliation

物質・材料研究機構

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

ROY Susmita,PRUSTI Banchhanidhi,SARKAR Shifa

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes

浦野 絵里

利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub),技術補助/Technical Assistance


利用した主な設備 / Equipment Used in This Project

NM-654:触針式プロファイラー [Dektak 6M]
NM-604:マスクレス露光装置 [DL-1000/NC2P]


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

Research and development of Electrochromic Dimmable Glass Devices is a huge attraction nowadays as window-modified materials in advanced buildings. They are capable of blocking solar radiation by altering their color from transparent-to-dark mode in the presence of applied bias. This leads to save a fraction of primary energy sources used in buildings for space cooling or ventilation. Therefore, our intention is to create a metal-organic assembly system, which could show transparent to dark EC. Creating a Fe-containing metal-organic assembly would be a great choice as Fe is an abundant material. So, we try to develop a Fe(III) based organo-metallic polymer system. To get a confirmation of synthesized compound and their structure it is necessary to go through some characterization technique like thickness measurement of film or FE-SEM to know the morphology confirmation.

実験 / Experimental

We have synthesized a dibromo-substituted Fe(II)NHC complex, which was dissolved in acetonitrile and spin-coated on ITO. Later the thickness and morphology were checked.

結果と考察 / Results and Discussion

To carry out the characterization, first, I took training for both the instrument, FE-SEM and Surface Profilometer. 
For training purpose and preliminary check, a different standard sample were checked in FE-SEM. So far, the synthesized compound was not checked as it was confirmed by other characterization technique like NMR.
For the thickness measurement, first for the training different sample were tested. Later, the I checked with my sample. The sample thickness was found to be ~270nm by surface profilometer.

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

  • 【更新日】0年0月0日
印刷する
PAGE TOP
スマートフォン用ページで見る