利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.04.22】

課題データ / Project Data

課題番号 / Project Issue Number

23NM5278

利用課題名 / Title

Hybrid nanocomposite materials for ORR applications

利用した実施機関 / Support Institute

物質・材料研究機構 / NIMS

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)物質・材料合成プロセス/Molecule & Material Synthesis

【重要技術領域 / Important Technology Area】(主 / Main)高度なデバイス機能の発現を可能とするマテリアル/Materials allowing high-level device functions to be performed(副 / Sub)次世代ナノスケールマテリアル/Next-generation nanoscale materials

キーワード / Keywords

ナノカーボン/ Nano carbon,ナノ多孔体/ Nanoporuous material,メソポーラス材料/ Mesoporous material


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

ヒル ジョナサン

所属名 / Affiliation

物質・材料研究機構

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)技術代行/Technology Substitution(副 / Sub),機器利用/Equipment Utilization


利用した主な設備 / Equipment Used in This Project

NM-202:硬X線光電子分光分析装置(HAX-PES/XPS)
NM-204:多目的X線回折装置_Cu_SSL
NM-647:FE-SEM+EDX [S-4800]


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

The aim of this work has been to prepare hybrid nanocomposite hierarchically porous nanomaterials for electrochemical applications especially as fuel cell electrode materials. 

実験 / Experimental

Materials were prepared by a combination of bottom-up (molecular synthesis) and top-down (carbonization) processes. The materials were characterized for electrode applications and their compositions were estimated using X-ray photoelectron spectroscopy, scanning electron microscopy (SEM/EDX) and powder X-ray diffraction.

結果と考察 / Results and Discussion

The materials were found to have excellent properties for oxygen reduction reaction applications. The electrochemical properties were similar to or better than the benchmark materials (Pt/C) depending on the synthesis method. The properties and economical preparation of these materials make them highly suitable as replacement materials of noble metal catalysts.

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
  1. Two papers under preparation for submission.
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件