利用報告書 / User's Reports

  • 印刷する

【公開日:2024.07.25】【最終更新日:2024.06.17】

課題データ / Project Data

課題番号 / Project Issue Number

23AT5030

利用課題名 / Title

ナノ結晶材料の合成

利用した実施機関 / Support Institute

産業技術総合研究所 / AIST

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者)/Internal Use (by ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)物質・材料合成プロセス/Molecule & Material Synthesis

【重要技術領域 / Important Technology Area】(主 / Main)革新的なエネルギー変換を可能とするマテリアル/Materials enabling innovative energy conversion(副 / Sub)高度なデバイス機能の発現を可能とするマテリアル/Materials allowing high-level device functions to be performed

キーワード / Keywords

量子効果デバイス/ Quantum effect device,太陽電池/ Solar cell


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

松井 卓矢

所属名 / Affiliation

産業技術総合研究所 再生可能エネルギー研究センター

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes

Vladimir Svrcek

ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes

松﨑弘幸 ,永井秀和

利用形態 / Support Type

(主 / Main)技術補助/Technical Assistance(副 / Sub)-


利用した主な設備 / Equipment Used in This Project

AT-503:可視-近赤外過渡吸収分光装置 (VITA)


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

To enhance the interaction with the host perovskite matrix and solar cell performance, we modify the surface and shape of both the perovskites and silicon quantum dots. Our approach involves utilizing femtosecond laser (fs laser) at wavelengths of 800 and 400 nm, varying the intensity as a key parameter.

実験 / Experimental

One representative experiment outcome is depicted in FIG. 1a below, obtained by focusing the fs laser beam at a wavelength of 400 nm on the solution containing SiQDs. The quantum dots (QDs) are dispersed in various solutions such as water, octane, and hexene.

結果と考察 / Results and Discussion

The laser-treated SiQDs are subsequently introduced to perovskites to fabricate solar cells. Figure 1b illustrates typical J-V curves of solar cells based on perovskite, with and without laser-treated SiQDs. It's evident that there's an enhancement in the IV characteristics upon the introduction of laser-treated SiQDs.  

図・表・数式 / Figures, Tables and Equations


Fig 1a) shows the laser treatment of SiQDs by focusing the fs laser beam at a wavelength of 400 nm on the solution containing SiQDs. Fig 1b) illustrates typical J-V curves of solar cells based on perovskite, with and without laser-treated SiQDs.


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
  1. Svrcek, Vladimir; McDonald, Calum; Padmanaban, Dilli Babu; McGlynn, Ruairi; Kambley, Ankur; Alessi, Bruno; Mariotti, Davide; Matsui, Takuya, "Benefits of Surface Engineered Silicon Quantum Dots in Formamidinium Lead Iodide Perovskite Solar Cells", 2023 IEEE 50th Photovoltaic Specialists Conference (PVSC), 2023.6