利用課題名 / Title

Fabrication and electro-mechanical study of nano-scale resonators

利用した実施機関 / Support Institute

京都大学 / Kyoto Univ.

機関外・機関内の利用 / External or Internal Use

内部利用(ARIM事業参画者以外)/Internal Use (by non ARIM members)

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)加工・デバイスプロセス/Nanofabrication(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)マルチマテリアル化技術・次世代高分子マテリアル/Multi-material technologies / Next-generation high-molecular materials(副 / Sub)高度なデバイス機能の発現を可能とするマテリアル/Materials allowing high-level device functions to be performed

キーワード / Keywords

Resonator, Nanomechanical engineering,リソグラフィ/Lithography,EB,3D積層技術/ 3D lamination technology


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Banerjee Amit

所属名 / Affiliation

京都大学 大学院工学研究科

共同利用者氏名 / Names of Collaborators in Other Institutes Than Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Collaborators in The Hub and Spoke Institutes

江崎裕子

利用形態 / Support Type

(主 / Main)機器利用/Equipment Utilization(副 / Sub),技術補助/Technical Assistance


利用した主な設備 / Equipment Used in This Project

KT-117:超臨界洗浄・乾燥装置


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

In this research, our goal is to fabricate nanoscale resonator devices of Si to study their dynamic behavior, Q-factor, etc. for developing ultrasensitive gas-sensors. This research is done together with Wei Yu, Yuma Ohara and Tsubasa Suzuki. Each of their individual research and reports are separately provided. I provide mentorship to their efforts regarding concepts and designs of devices, fabrication process and optimizing process conditions. As far as my personal use of equipment in this issue, I used the critical point dryer to dry a few nanoresonator chips after acetone cleaning. Details of that experiment is provided below. For further detail about this research and achievements, I refer to the reports of the aforementioned student members of the project. 

実験 / Experimental

We fabricate our nanoresonator devices from SOI wafers using UV and electron beam lithography, DRIE process and vapor HF etching. In some of our devices, due to over-etching in DRIE step, nanobeams were detached from the oxide layer. In the next step, when some of the chips were diced and protective photoresist layer was removed by acetone, nanobeams were damaged during drying. To overcome this issue, I used critical point drying (KT-117: Supercritical Rinser & Dryer) to dry the remaining chips after 15 minutes acetone cleaning.

結果と考察 / Results and Discussion

Chips were inspected under an optical microscope before and after the critical points drying process as shown in Fig. 1(a) and Fig. 1(b), respectively. In Fig. 1(a), photoresist (OFPR) coating is visible on the chip. Fig. 1(b) shows a chip after resist removal and drying process with intact nanobeams, indicating that the beams were successfully rescued.

図・表・数式 / Figures, Tables and Equations


Fig.1: Optical images of devices (a) before and (b) after critical point drying.


その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)


成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
  1. 2022 JSME-IIP/ASME-ISPS Joint Conference on Micromechatronics for Information and Precision Equipment, Nagoya, Aug 2022
特許 / Patents

特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件

  • 【更新日】0年0月0日
印刷する
PAGE TOP
スマートフォン用ページで見る