利用報告書 / User's Reports

  • 印刷する

【公開日:2025.07.10】【最終更新日:2025.07.10】

課題データ / Project Data

課題番号 / Project Issue Number

22UT0396

利用課題名 / Title

Catalysis by supported bimetallic particles on modified mesoporous silica

利用した実施機関 / Support Institute

東京大学 / Tokyo Univ.

機関外・機関内の利用 / External or Internal Use

外部利用/External Use

技術領域 / Technology Area

【横断技術領域 / Cross-Technology Area】(主 / Main)計測・分析/Advanced Characterization(副 / Sub)-

【重要技術領域 / Important Technology Area】(主 / Main)次世代ナノスケールマテリアル/Next-generation nanoscale materials(副 / Sub)-

キーワード / Keywords

catalyst、alloy particles,電子顕微鏡/Electron microscopy,ナノ粒子/ Nanoparticles


利用者と利用形態 / User and Support Type

利用者名(課題申請者)/ User Name (Project Applicant)

Etty Nurlia Kusumawati

所属名 / Affiliation

岩手大学理工学部 化学・生命理工学科

共同利用者氏名 / Names of Collaborators Excluding Supporters in the Hub and Spoke Institutes
ARIM実施機関支援担当者 / Names of Supporters in the Hub and Spoke Institutes
利用形態 / Support Type

(主 / Main)技術補助/Technical Assistance(副 / Sub),技術相談/Technical Consultation


利用した主な設備 / Equipment Used in This Project

UT-005:原子分解能元素マッピング構造解析装置


報告書データ / Report

概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)

The purpose of this study is to develop supported bimetallic catalysts in which ionic liquids (ILs) are immobilized on mesoporous silica SBA-15 and to study their structural properties in hydrogenation reactions. To understand therelationship between structural properties and reactivity, it is important to identify their characteristic properties. For this purpose, STEM characterization was performed, and the formation of alloy particles was confirmed.

実験 / Experimental

STEM images and EDS elemental mappings of the prepared Pt-Co/IL@SBA-15 were taken using JEM-ARM200F Thermal

結果と考察 / Results and Discussion

The formation of small bimetallic Pt-Co particles on the Pt-Co/IL@SBA-15 sample was confirmed from the STEM-EDS mapping images. Small bimetallic particles with enriched Pt-Co surfaces were mostly observed inside the pores of SBA-15.

図・表・数式 / Figures, Tables and Equations
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)



成果発表・成果利用 / Publication and Patents

論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
  1. E.N. Kusumawati, T. Sasaki, M. Shirai, “Pt-Co Bimetallic Catalyst Containing Immobilized Ionic Liquid on SBA-15 for Solvent-Free Hydrogenation of Cinnamaldehyde”, 第131 回触媒討論会, 15-17 March 2023