【公開日:2025.07.07】【最終更新日:2025.07.04】
課題データ / Project Data
課題番号 / Project Issue Number
22NI5502
利用課題名 / Title
Synthesis and characterization of carbon nanomaterials
利用した実施機関 / Support Institute
名古屋工業大学 / Nagoya Tech.
機関外・機関内の利用 / External or Internal Use
外部利用/External Use
技術領域 / Technology Area
【横断技術領域 / Cross-Technology Area】(主 / Main)物質・材料合成プロセス/Molecule & Material Synthesis(副 / Sub)計測・分析/Advanced Characterization
【重要技術領域 / Important Technology Area】(主 / Main)マテリアルの高度循環のための技術/Advanced materials recycling technologies(副 / Sub)高度なデバイス機能の発現を可能とするマテリアル/Materials allowing high-level device functions to be performed
キーワード / Keywords
Carbon related materials,電子顕微鏡/Electron microscopy,ナノエレクトロニクスデバイス/ Nanoelectronics device,易循環型材料設計技術/ Recycling-friendly material design technology
利用者と利用形態 / User and Support Type
利用者名(課題申請者)/ User Name (Project Applicant)
Hilmi Ibrahim
所属名 / Affiliation
Universiti Teknologi Malaysia (UTM)
共同利用者氏名 / Names of Collaborators Excluding Supporters in the Hub and Spoke Institutes
Mohd Fairus Mohd Yasin,Mohd Zamri Mohd Yusop
ARIM実施機関支援担当者 / Names of Supporters in the Hub and Spoke Institutes
Masaki Tanemura,Yazid Yaakob
利用形態 / Support Type
(主 / Main)共同研究/Joint Research(副 / Sub)-
利用した主な設備 / Equipment Used in This Project
NI-106:グラフェン・カーボンナノチューブ合成装置
NI-001:原子分解能分析電子顕微鏡群
報告書データ / Report
概要(目的・用途・実施内容)/ Abstract (Aim, Use Applications and Contents)
The synthesis of carbon nanotubes (CNTs) and their characterization using transmission electron microscopy (TEM) were carried out in Nagoya Institute of Technology (NITech). The results of the characterization will be analyzed also in the High Speed Reacting Flow Laboratory (HiREF) lab in Universiti Teknologi Malaysia (UTM) in terms of graphitic structure and tubular size. In addition, a comparative analysis will be conducted against the commercially-purchased products of similar properties.
実験 / Experimental
The CNT samples thus synthesized were in the powder form. They were transferred to the aberration-corrected electron microscope (JEM-ARM200F) for their structural analysis.
結果と考察 / Results and Discussion
The typical crystalline structure and numbers of the walls of the synthesized CNTs are summarized in Fig. 1. They were categorized into tubular (multiwall), herringbone, and bamboo structures depending on the synthesis conditions.
図・表・数式 / Figures, Tables and Equations
Fig.1 TEM images of the crystalline structure and numbers of the walls of the synthesized CNTs
その他・特記事項(参考文献・謝辞等) / Remarks(References and Acknowledgements)
Thanks to Yazid Yaakob and Masaki Tanemura (NITech).
成果発表・成果利用 / Publication and Patents
論文・プロシーディング(DOIのあるもの) / DOI (Publication and Proceedings)
口頭発表、ポスター発表および、その他の論文 / Oral Presentations etc.
特許 / Patents
特許出願件数 / Number of Patent Applications:0件
特許登録件数 / Number of Registered Patents:0件