データセット名:Observation of atomic arrangement at the heterojunction interface of high temperature superconductor heterostructures

課題名:Observation of atomic arrangement at the heterojunction interface of high temperature superconductor heterostructures

データセット登録者(所属機関):JIA, Jiqiang (Xi'an university os techology)

課題番号:
JPMXP1222JI0053
実施機関:
北陸先端科学技術大学院大学

要約

The purpose of this project is to study the influence of the growth characteristics and interface arrangement of atoms on the electromagnetism properties of heterostructures formed by two different superconductors. In the experiment, YBa2Cu3O7-δ/Nd1.85Ce0.15CuO4 (YBCO/NCCO) hetero structure grown on SrTiO3 (STO) substrate was observed using the spherical aberration corrected transmission electron microscope (JEM-ARM200F). The atomic arrangement and material growth orientation at the YBCO/NCCO interface was studied, and the bright field and high-angle annular dark field images of the above interfaces were obtained

162e512f-fc58-4caf-a66d-d4669fc70000
05176e5a-83c4-42fe-8a8a-a16301f85c45
dc0c7d2f-9b54-4294-893b-5269480bf23e

キーワード・タグ

重要技術領域(主):
重要技術領域(副):
横断技術領域:
マテリアルインデックス:
キーワードタグ:

データメトリックス

ページビュー:
155
ダウンロード数:
0

データインデックス

https://doi.org/10.71947/arim.jpmxp1222ji0053
登録日:
2025.04.17
エンバーゴ解除日:
2025.03.31
データセットID:
94912117-9a4b-4c96-bca4-84d699c8b666
データタイル数:
3
ファイル数:
149
ファイルサイズ:
481.45MB
ライセンス:
ARIMライセンス

成果発表・成果利用